High velocity air fuel spraying of nickel titanium coatings: microstructure, phase transformation and shape memory behavior

Published:
Updated:
Views: --

1 Research Foundations

1.1 Research Context and Motivation

The paper is organized as an experimental materials processing study. Its central method is to deposit thick nickel titanium coatings on steel using high velocity air fuel thermal spraying, then characterize whether those coatings preserve the functional thermomechanical behavior associated with shape memory alloys. The novelty lies in treating coating fabrication and functional testing as one connected workflow.

The starting material is pre alloyed nickel titanium powder with near equiatomic composition. The powder is characterized before spraying because its particle size, morphology, chemistry, and transformation temperatures set the baseline for interpreting the coatings. Differential scanning calorimetry shows that the powder itself undergoes martensitic transformation, which provides a reference for later coating changes.

The coatings are deposited on grit blasted mild steel substrates. Grit blasting creates surface roughness that promotes mechanical interlocking and adhesion during spraying. The authors use two nozzle configurations and four sets of process parameters, varying nozzle type, air pressure, and coating thickness while keeping carrier gas and powder feed conditions controlled.

1.2 Methodological Framework

The use of high velocity air fuel spraying is methodologically important because conventional plasma spraying can overheat nickel titanium and produce chemically inhomogeneous coatings, while cold spraying can suffer from weak adhesion. The selected process aims to deliver particles with enough velocity for bonding while limiting thermal damage that would suppress transformation behavior.

Phase composition is measured by X ray diffraction at room temperature. The authors compare the powder diffraction pattern with the patterns of all four coatings and use quantitative refinement to estimate phase fractions and lattice parameters. This step tests whether spraying changes the balance between austenite, martensite, oxides, or other phases.

Microstructure is examined by scanning electron microscopy and chemical analysis. The paper looks for porosity, oxide particles, deformation features, and compositional heterogeneity across the coating. These observations are not only descriptive: they explain why transformation temperatures and mechanical performance differ from the starting powder and from bulk nickel titanium.

2 Evidence and Interpretation

2.1 Evidence and Evaluation

The authors explicitly connect process parameters to coating properties. Four coating conditions are produced so that the sensitivity of microstructure, porosity, phase composition, and mechanical response can be compared. This comparative design is necessary because a single successful coating would not reveal which fabrication choices control functional behavior.

Thermal transformation behavior is evaluated after spraying and after annealing. As sprayed coatings are largely austenitic at room temperature and may have suppressed transformation because of deformation, residual stress, or composition changes caused by oxidation. Annealing is therefore treated as part of the processing route rather than as an optional postscript.

Mechanical and functional performance is assessed with several complementary tests. Tensile or adhesion related observations indicate whether the coating remains attached and structurally usable, while three point bending tests examine thermal actuation. Nanoindentation and scratch tests probe local shape memory or recovery behavior at smaller scales within the coating.

2.2 Interpretation and Reproducibility

The paper pays attention to adhesion because a functional coating has little engineering value if it separates from the substrate. The grit blasted steel surface and high velocity impact are intended to improve bonding. The characterization therefore considers not only transformation but also whether the coating can survive handling and mechanical loading.

Porosity and internal defects are treated as unavoidable but measurable consequences of the spraying process. Voids, oxide inclusions, dislocation density, and residual stress can weaken the coating, but they do not necessarily eliminate martensitic transformation. The method evaluates how much functional behavior remains despite these microstructural imperfections.

The annealing experiments provide a key interpretation step. If functional behavior improves after heat treatment, then the limitation of as sprayed coatings is not simply incorrect chemistry; it is also connected to internal stress, deformation defects, and recoverable microstructural states. This guides future optimization of spray and post treatment parameters.

3 Conclusions and Outlook

3.1 Limitations and Key Takeaways

The work also identifies appropriate characterization methods for future process optimization. X ray diffraction tracks phase state, microscopy reveals defects and chemistry, calorimetry detects transformation temperatures, and mechanical tests reveal actuation or recovery. The method is therefore a toolkit for deciding whether a sprayed nickel titanium coating is genuinely functional.

The main evidence for success is not that the coatings are defect free. Instead, the paper shows that thick coatings with imperfect and heterogeneous microstructures can still undergo martensitic transformation and display thermal actuation or shape memory effects after suitable treatment. This is a practical standard for coating applications rather than an idealized bulk alloy standard.

The main limitation is mechanical strength. The coatings can adhere and show functional response, but their tensile performance is limited by porosity, oxides, and internal defects. The methodological contribution is therefore a fabrication and characterization route that demonstrates feasibility while also identifying the microstructural obstacles that future high velocity spraying studies must reduce.